As the PV industry scales to annual terawatt-level production to rapidly curtail the world’s emissions, it will become more challenging to continue the cost reduction trajectory. Increasing module ...
Fraunhofer ISE development also uses recyclable aluminum for masking – removing need for problem polymers. Thin copper contacts mean the silicon layer does not experience much shading. The rising ...
Trilyte Dusk trivalent-chromium plating process deposits a dark, lustrous, repeatable chromium layer over bright or satin nickel deposits. The coating passes 80 hr of exposure to acetic acid with ...
Researchers at the University of New South Wales have used a 1 µm copper plating layer on the front silver grid of a TOPCon solar cell to create a protective barrier that reportedly reduces corrosion ...